A study on stress-corrosion cracking using single fiber model specimen (degradation properties of GFRP caused by water absorption)

Hiroyuki Kawada, Akira Kobiki

Research output: Contribution to journalArticlepeer-review

7 Citations (Scopus)

Fingerprint Dive into the research topics of 'A study on stress-corrosion cracking using single fiber model specimen (degradation properties of GFRP caused by water absorption)'. Together they form a unique fingerprint.

Chemical Compounds

Engineering & Materials Science