    The objective of this study is to clarify dissolution behavior of duplex stainless steels in crevice corrosion growth step. Crevice corrosion grew on the duplex stainless steels by holding potential at various values. After a certain period, dissolution behavior of the crevice corrosion was analyzed based on observation of corroded area. Change in crevice corrosion dissolution behavior with time was also investigated by means of in-situ observation. Four types of dissolution regions could be observed in the corrosion area from outside toward inside direction, i.e., tip of the corroded area toward initiation point, in a crevice; they were passive region, the preferential dissolution region of γ phase, α phase and γ phase dissolution region, and the preferential dissolution region of α phase. The crevice corrosion which maintained that four dissolution regions grew toward the edge of the crevice. This dissolution behavior was given at all the potential where crevice corrosion occurred.

    Original languageEnglish
    Pages (from-to)366-372
    Number of pages7
    JournalZairyo to Kankyo/ Corrosion Engineering
    Volume64
    Issue number8
    Publication statusPublished - 2015

    Fingerprint

    Stainless Steel
    Dissolution
    Stainless steel
    Corrosion

    Keywords

    • Crevice corrosion
    • Duplex stainless steel
    • In-situ observation
    • IR drop
    • Potentiostatic test
    • Preferential dissolution

    ASJC Scopus subject areas

    • Electrochemistry
    • Materials Chemistry
    • Metals and Alloys
    • Surfaces, Coatings and Films

    Cite this

    Dissolution Behavior of Duplex Stainless Steels in Crevice Corrosion Growth Step. / Aoki, So; Nada, Yushi; Sakai, Jun'Ichi.

    In: Zairyo to Kankyo/ Corrosion Engineering, Vol. 64, No. 8, 2015, p. 366-372.

    Research output: Contribution to journalArticle

    Aoki, So ; Nada, Yushi ; Sakai, Jun'Ichi. / Dissolution Behavior of Duplex Stainless Steels in Crevice Corrosion Growth Step. In: Zairyo to Kankyo/ Corrosion Engineering. 2015 ; Vol. 64, No. 8. pp. 366-372.
    @article{296ac1fa5ffe4bb9bae4adc1ef97996b,
    title = "Dissolution Behavior of Duplex Stainless Steels in Crevice Corrosion Growth Step",
    abstract = "The objective of this study is to clarify dissolution behavior of duplex stainless steels in crevice corrosion growth step. Crevice corrosion grew on the duplex stainless steels by holding potential at various values. After a certain period, dissolution behavior of the crevice corrosion was analyzed based on observation of corroded area. Change in crevice corrosion dissolution behavior with time was also investigated by means of in-situ observation. Four types of dissolution regions could be observed in the corrosion area from outside toward inside direction, i.e., tip of the corroded area toward initiation point, in a crevice; they were passive region, the preferential dissolution region of γ phase, α phase and γ phase dissolution region, and the preferential dissolution region of α phase. The crevice corrosion which maintained that four dissolution regions grew toward the edge of the crevice. This dissolution behavior was given at all the potential where crevice corrosion occurred.",
    keywords = "Crevice corrosion, Duplex stainless steel, In-situ observation, IR drop, Potentiostatic test, Preferential dissolution",
    author = "So Aoki and Yushi Nada and Jun'Ichi Sakai",
    year = "2015",
    language = "English",
    volume = "64",
    pages = "366--372",
    journal = "Corrosion Engineering",
    issn = "0917-0480",
    publisher = "Japan Society of Corrosion Engineering",
    number = "8",

    }

    TY - JOUR

    T1 - Dissolution Behavior of Duplex Stainless Steels in Crevice Corrosion Growth Step

    AU - Aoki, So

    AU - Nada, Yushi

    AU - Sakai, Jun'Ichi

    PY - 2015

    Y1 - 2015

    N2 - The objective of this study is to clarify dissolution behavior of duplex stainless steels in crevice corrosion growth step. Crevice corrosion grew on the duplex stainless steels by holding potential at various values. After a certain period, dissolution behavior of the crevice corrosion was analyzed based on observation of corroded area. Change in crevice corrosion dissolution behavior with time was also investigated by means of in-situ observation. Four types of dissolution regions could be observed in the corrosion area from outside toward inside direction, i.e., tip of the corroded area toward initiation point, in a crevice; they were passive region, the preferential dissolution region of γ phase, α phase and γ phase dissolution region, and the preferential dissolution region of α phase. The crevice corrosion which maintained that four dissolution regions grew toward the edge of the crevice. This dissolution behavior was given at all the potential where crevice corrosion occurred.

    AB - The objective of this study is to clarify dissolution behavior of duplex stainless steels in crevice corrosion growth step. Crevice corrosion grew on the duplex stainless steels by holding potential at various values. After a certain period, dissolution behavior of the crevice corrosion was analyzed based on observation of corroded area. Change in crevice corrosion dissolution behavior with time was also investigated by means of in-situ observation. Four types of dissolution regions could be observed in the corrosion area from outside toward inside direction, i.e., tip of the corroded area toward initiation point, in a crevice; they were passive region, the preferential dissolution region of γ phase, α phase and γ phase dissolution region, and the preferential dissolution region of α phase. The crevice corrosion which maintained that four dissolution regions grew toward the edge of the crevice. This dissolution behavior was given at all the potential where crevice corrosion occurred.

    KW - Crevice corrosion

    KW - Duplex stainless steel

    KW - In-situ observation

    KW - IR drop

    KW - Potentiostatic test

    KW - Preferential dissolution

    UR - http://www.scopus.com/inward/record.url?scp=84960077512&partnerID=8YFLogxK

    UR - http://www.scopus.com/inward/citedby.url?scp=84960077512&partnerID=8YFLogxK

    M3 - Article

    AN - SCOPUS:84960077512

    VL - 64

    SP - 366

    EP - 372

    JO - Corrosion Engineering

    JF - Corrosion Engineering

    SN - 0917-0480

    IS - 8

    ER -