Surface analysis and biocorrosion properties of nanostructured surface sol-gel coatings on Ti6Al4V titanium alloy implants

Maria C. Advincula, Don Petersen, Firoz Rahemtulla, Rigoberto Advincula, Jack E. Lemons

Research output: Contribution to journalArticlepeer-review