Analyses on a declining performance of PEMFC with fuel containing impurities (2nd report, characteristic evaluation of methanol reforming type fuel cells)

Kazuyuki Narusawa*, Morimasa Hayashida, Daisuke Kurashima, Kenji Murooka, Katsuhiko Wakabayashi, Yushi Kamiya

*この研究の対応する著者

研究成果: Article査読

3 被引用数 (Scopus)

抄録

This paper covers our investigation into a decline in performance resulting from use of fuel containing impurities in methanol reforming type FCs. The investigations conducted and their results are as follows: 1) Various experiments and analyses were conducted to determine the adverse effects of CO, HCHO, HCOOH, and CH4 on the performance of the FC; 2) In the case of HCHO and HCOOH poisoning, performance became worse when Ru was added to the FC catalytic-electrode; 3) The quantities of the partial pressure decline phenomenon of hydrogen gas caused by mixing CO2 and N2 gases appeared to be the same; 4) The progress of poisoning with the reforming gas was complex; however, explanation became possible by taking CO poisoning and the influence of the partial pressure decline phenomenon of hydrogen gas into consideration.

本文言語English
ページ(範囲)2553-2559
ページ数7
ジャーナルNippon Kikai Gakkai Ronbunshu, B Hen/Transactions of the Japan Society of Mechanical Engineers, Part B
69
687
DOI
出版ステータスPublished - 2003 11月
外部発表はい

ASJC Scopus subject areas

  • 凝縮系物理学
  • 機械工学

フィンガープリント

「Analyses on a declining performance of PEMFC with fuel containing impurities (2nd report, characteristic evaluation of methanol reforming type fuel cells)」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。