抄録
The correlation between degradation-induced changes in two important indicators of mechanical properties, namely elongation at break (EAB) and indenter modulus (IM), is examined for flame-retardant ethylene propylene rubber (FR-EPR), silicone rubber (SiR), flame-retardant crosslinked polyethylene (FR-XLPE), and XLPE. The samples were degraded by heat or concurrently by heat and radiation. In the case that the polymers become hard after they were degraded, the two indicators show a good correlation. However, if they become brittle, their correlation is not good. Regarding this, their correlation is good in SiR, while it is not good in FR-XLPE and XLPE. In FR-EPR, the correlativity changes, depending on the aging condition and presumably its additives.
本文言語 | English |
---|---|
ホスト出版物のタイトル | Proceedings of 2017 International Symposium on Electrical Insulating Materials, ISEIM 2017 |
出版社 | Institute of Electrical Engineers of Japan |
ページ | 753-756 |
ページ数 | 4 |
巻 | 2 |
ISBN(電子版) | 9784886860996 |
DOI | |
出版ステータス | Published - 2017 12月 4 |
イベント | 2017 International Symposium on Electrical Insulating Materials, ISEIM 2017 - Toyohashi, Japan 継続期間: 2017 9月 11 → 2017 9月 15 |
Other
Other | 2017 International Symposium on Electrical Insulating Materials, ISEIM 2017 |
---|---|
国/地域 | Japan |
City | Toyohashi |
Period | 17/9/11 → 17/9/15 |
ASJC Scopus subject areas
- 電子工学および電気工学
- 電子材料、光学材料、および磁性材料