Crystalline-oriented TiO2 fabricated by the electrophoretic deposition in a strong magnetic field

T. Uchikoshi*, T. S. Suzuki, F. Tang, H. Okuyama, Y. Sakka

*この研究の対応する著者

研究成果: Conference article査読

35 被引用数 (Scopus)

抄録

Electrophoretic deposition of titania (anatase) suspension was conducted in a strong magnetic field of 10T. The direction of the electric field E relative to the magnetic field B was altered (φB-E=0, 30, 60 and 90°) to control the dominant crystal faces of the deposit surfaces. The crystalline orientation was investigated by the X-ray diffraction for the titania films of as-deposited, sintered at 650, 750 and 1200°C as a function of the angle between the directions of B and E (φB-E). It was found that changing the angle φB-E during the EPD could control the crystalline orientation of the titania films.

本文言語English
ページ(範囲)1975-1978
ページ数4
ジャーナルCeramics International
30
7
DOI
出版ステータスPublished - 2004
外部発表はい
イベント3rd Asian Meeting on Electroceramics - Singapore, Singapore
継続期間: 2003 12月 72003 12月 11

ASJC Scopus subject areas

  • 電子材料、光学材料、および磁性材料
  • セラミックおよび複合材料
  • プロセス化学およびプロセス工学
  • 表面、皮膜および薄膜
  • 材料化学

フィンガープリント

「Crystalline-oriented TiO2 fabricated by the electrophoretic deposition in a strong magnetic field」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル