    抄録

    The practical lifetime of a polymeric insulating material is determined in most cases by its partial discharge resistance at an operating temperature. Therefore, in this research, the partial discharge resistance was examined for eight kinds of polymer samples. An ac 500-Hz voltage with a designated value was applied to a sample sheet sandwiched between a pair of IEC (b) electrodes at 353K and 30% relative humidity for a designated period. The sheet surface degraded by partial discharges was then observed by a mechanical surface profilometer to measure the shape, from which the whole eroded volume was estimated. As a result, it has been clarified that polymers can exhibit superior partial discharge resistance when their melting point, molecular weight of chain repeating unit, density, weight ratio of benzene rings, and crystallinity are high.

    元の言語English
    ホスト出版物のタイトルProceedings of the IEEE International Conference on Properties and Applications of Dielectric Materials
    DOI
    出版物ステータスPublished - 2012
    イベント2012 IEEE 10th International Conference on the Properties and Applications of Dielectric Materials, ICPADM 2012 - Bangalore
    継続期間: 2012 7 242012 7 28

    Other

    Other2012 IEEE 10th International Conference on the Properties and Applications of Dielectric Materials, ICPADM 2012
    Bangalore
    期間12/7/2412/7/28

    Fingerprint

    Partial discharges
    Polymers
    polymers
    profilometers
    Insulating materials
    Benzene
    operating temperature
    insulation
    melting points
    Melting point
    humidity
    molecular weight
    crystallinity
    Atmospheric humidity
    Molecular weight
    benzene
    life (durability)
    Electrodes
    electrodes
    rings

    ASJC Scopus subject areas

    • Electronic, Optical and Magnetic Materials
    • Materials Chemistry
    • Condensed Matter Physics

    これを引用

    Hasegawa, Y., Isamu, I., & Ohki, Y. (2012). Experimental study on the factors determining the partial discharge resistance of polymers. : Proceedings of the IEEE International Conference on Properties and Applications of Dielectric Materials [6318947] https://doi.org/10.1109/ICPADM.2012.6318947

    Experimental study on the factors determining the partial discharge resistance of polymers. / Hasegawa, Yuka; Isamu, Ikeda; Ohki, Yoshimichi.

    Proceedings of the IEEE International Conference on Properties and Applications of Dielectric Materials. 2012. 6318947.

    研究成果: Conference contribution

    Hasegawa, Y, Isamu, I & Ohki, Y 2012, Experimental study on the factors determining the partial discharge resistance of polymers. : Proceedings of the IEEE International Conference on Properties and Applications of Dielectric Materials., 6318947, 2012 IEEE 10th International Conference on the Properties and Applications of Dielectric Materials, ICPADM 2012, Bangalore, 12/7/24. https://doi.org/10.1109/ICPADM.2012.6318947
    Hasegawa Y, Isamu I, Ohki Y. Experimental study on the factors determining the partial discharge resistance of polymers. : Proceedings of the IEEE International Conference on Properties and Applications of Dielectric Materials. 2012. 6318947 https://doi.org/10.1109/ICPADM.2012.6318947
    Hasegawa, Yuka ; Isamu, Ikeda ; Ohki, Yoshimichi. / Experimental study on the factors determining the partial discharge resistance of polymers. Proceedings of the IEEE International Conference on Properties and Applications of Dielectric Materials. 2012.
    @inproceedings{e0c3cd1c94de4468bd8b5c3c9c3e2b46,
    title = "Experimental study on the factors determining the partial discharge resistance of polymers",
    abstract = "The practical lifetime of a polymeric insulating material is determined in most cases by its partial discharge resistance at an operating temperature. Therefore, in this research, the partial discharge resistance was examined for eight kinds of polymer samples. An ac 500-Hz voltage with a designated value was applied to a sample sheet sandwiched between a pair of IEC (b) electrodes at 353K and 30{\%} relative humidity for a designated period. The sheet surface degraded by partial discharges was then observed by a mechanical surface profilometer to measure the shape, from which the whole eroded volume was estimated. As a result, it has been clarified that polymers can exhibit superior partial discharge resistance when their melting point, molecular weight of chain repeating unit, density, weight ratio of benzene rings, and crystallinity are high.",
    keywords = "Engineering Plastics, Partial Discharge, Polyvinyl Polymers, Syndiotactic Polystyrene",
    author = "Yuka Hasegawa and Ikeda Isamu and Yoshimichi Ohki",
    year = "2012",
    doi = "10.1109/ICPADM.2012.6318947",
    language = "English",
    isbn = "9781467328500",
    booktitle = "Proceedings of the IEEE International Conference on Properties and Applications of Dielectric Materials",

    }

    TY - GEN

    T1 - Experimental study on the factors determining the partial discharge resistance of polymers

    AU - Hasegawa, Yuka

    AU - Isamu, Ikeda

    AU - Ohki, Yoshimichi

    PY - 2012

    Y1 - 2012

    N2 - The practical lifetime of a polymeric insulating material is determined in most cases by its partial discharge resistance at an operating temperature. Therefore, in this research, the partial discharge resistance was examined for eight kinds of polymer samples. An ac 500-Hz voltage with a designated value was applied to a sample sheet sandwiched between a pair of IEC (b) electrodes at 353K and 30% relative humidity for a designated period. The sheet surface degraded by partial discharges was then observed by a mechanical surface profilometer to measure the shape, from which the whole eroded volume was estimated. As a result, it has been clarified that polymers can exhibit superior partial discharge resistance when their melting point, molecular weight of chain repeating unit, density, weight ratio of benzene rings, and crystallinity are high.

    AB - The practical lifetime of a polymeric insulating material is determined in most cases by its partial discharge resistance at an operating temperature. Therefore, in this research, the partial discharge resistance was examined for eight kinds of polymer samples. An ac 500-Hz voltage with a designated value was applied to a sample sheet sandwiched between a pair of IEC (b) electrodes at 353K and 30% relative humidity for a designated period. The sheet surface degraded by partial discharges was then observed by a mechanical surface profilometer to measure the shape, from which the whole eroded volume was estimated. As a result, it has been clarified that polymers can exhibit superior partial discharge resistance when their melting point, molecular weight of chain repeating unit, density, weight ratio of benzene rings, and crystallinity are high.

    KW - Engineering Plastics

    KW - Partial Discharge

    KW - Polyvinyl Polymers

    KW - Syndiotactic Polystyrene

    UR - http://www.scopus.com/inward/record.url?scp=84869452073&partnerID=8YFLogxK

    UR - http://www.scopus.com/inward/citedby.url?scp=84869452073&partnerID=8YFLogxK

    U2 - 10.1109/ICPADM.2012.6318947

    DO - 10.1109/ICPADM.2012.6318947

    M3 - Conference contribution

    AN - SCOPUS:84869452073

    SN - 9781467328500

    BT - Proceedings of the IEEE International Conference on Properties and Applications of Dielectric Materials

    ER -