Lotus-type porous Al-Si (4, 8, 12, 14, and 18 wt pct) alloys were fabricated using the continuous casting technique under a hydrogen gas pressure of 0.1 MPa at various transference velocities, and the effects of the silicon content level and transference velocity on the pore morphology and porosity were investigated. Both the porosity and the average pore diameter increase as the silicon content level increases and decrease as the transference velocity increases. In particular, the velocity dependence is obviously exhibited at a silicon content level higher than 12 wt pct. The pore shape is changed from irregular in the higher-dendrite fraction to nearly circular in the lower-dendrite fraction. The porosity and the pore morphology are influenced by the silicon content level and transference velocity. In the model, these results can be understood with the explanation that the pores, which contribute to the increase in porosity, are generated at the eutectic fronts. This indicated that the porosity and the pore size in lotus-type porous Al-Si alloys can be well controlled by varying the silicon content level and the transference velocity.

元の言語English
ページ(範囲)406-414
ページ数9
ジャーナルMetallurgical and Materials Transactions A: Physical Metallurgy and Materials Science
40
発行部数2
DOI
出版物ステータスPublished - 2009
外部発表Yes

Fingerprint

Continuous casting
Silicon
porosity
Fabrication
Porosity
fabrication
silicon
dendrites
Eutectics
Pore size
Hydrogen
Gases
eutectics
gas pressure

ASJC Scopus subject areas

  • Condensed Matter Physics
  • Metals and Alloys
  • Mechanics of Materials

これを引用

@article{5e249b0c8c7d4687a89e56622a9e542f,
title = "Fabrication of lotus-type porous Al-Si alloys using the continuous casting technique",
abstract = "Lotus-type porous Al-Si (4, 8, 12, 14, and 18 wt pct) alloys were fabricated using the continuous casting technique under a hydrogen gas pressure of 0.1 MPa at various transference velocities, and the effects of the silicon content level and transference velocity on the pore morphology and porosity were investigated. Both the porosity and the average pore diameter increase as the silicon content level increases and decrease as the transference velocity increases. In particular, the velocity dependence is obviously exhibited at a silicon content level higher than 12 wt pct. The pore shape is changed from irregular in the higher-dendrite fraction to nearly circular in the lower-dendrite fraction. The porosity and the pore morphology are influenced by the silicon content level and transference velocity. In the model, these results can be understood with the explanation that the pores, which contribute to the increase in porosity, are generated at the eutectic fronts. This indicated that the porosity and the pore size in lotus-type porous Al-Si alloys can be well controlled by varying the silicon content level and the transference velocity.",
author = "Park, {J. S.} and Hyun, {S. K.} and Shinsuke Suzuki and H. Nakajima",
year = "2009",
doi = "10.1007/s11661-008-9710-3",
language = "English",
volume = "40",
pages = "406--414",
journal = "Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science",
issn = "1073-5623",
publisher = "Springer Boston",
number = "2",

}

TY - JOUR

T1 - Fabrication of lotus-type porous Al-Si alloys using the continuous casting technique

AU - Park, J. S.

AU - Hyun, S. K.

AU - Suzuki, Shinsuke

AU - Nakajima, H.

PY - 2009

Y1 - 2009

N2 - Lotus-type porous Al-Si (4, 8, 12, 14, and 18 wt pct) alloys were fabricated using the continuous casting technique under a hydrogen gas pressure of 0.1 MPa at various transference velocities, and the effects of the silicon content level and transference velocity on the pore morphology and porosity were investigated. Both the porosity and the average pore diameter increase as the silicon content level increases and decrease as the transference velocity increases. In particular, the velocity dependence is obviously exhibited at a silicon content level higher than 12 wt pct. The pore shape is changed from irregular in the higher-dendrite fraction to nearly circular in the lower-dendrite fraction. The porosity and the pore morphology are influenced by the silicon content level and transference velocity. In the model, these results can be understood with the explanation that the pores, which contribute to the increase in porosity, are generated at the eutectic fronts. This indicated that the porosity and the pore size in lotus-type porous Al-Si alloys can be well controlled by varying the silicon content level and the transference velocity.

AB - Lotus-type porous Al-Si (4, 8, 12, 14, and 18 wt pct) alloys were fabricated using the continuous casting technique under a hydrogen gas pressure of 0.1 MPa at various transference velocities, and the effects of the silicon content level and transference velocity on the pore morphology and porosity were investigated. Both the porosity and the average pore diameter increase as the silicon content level increases and decrease as the transference velocity increases. In particular, the velocity dependence is obviously exhibited at a silicon content level higher than 12 wt pct. The pore shape is changed from irregular in the higher-dendrite fraction to nearly circular in the lower-dendrite fraction. The porosity and the pore morphology are influenced by the silicon content level and transference velocity. In the model, these results can be understood with the explanation that the pores, which contribute to the increase in porosity, are generated at the eutectic fronts. This indicated that the porosity and the pore size in lotus-type porous Al-Si alloys can be well controlled by varying the silicon content level and the transference velocity.

UR - http://www.scopus.com/inward/record.url?scp=59149095692&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=59149095692&partnerID=8YFLogxK

U2 - 10.1007/s11661-008-9710-3

DO - 10.1007/s11661-008-9710-3

M3 - Article

AN - SCOPUS:59149095692

VL - 40

SP - 406

EP - 414

JO - Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science

JF - Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science

SN - 1073-5623

IS - 2

ER -