Novel selectively sulfonated graft copolymers, poly(methyl methacrylate)-g-(poly(sulfonic acid styrene)-b-poly(tert-butylstyrene)), poly(methyl methacrylate)-g-(poly(tert-butylstyrene)-b-poly(styrenesulfonic acid)), and the corresponding sodium sulfonate salts were successfully synthesized. The weight-average molecular weights (Mw) of the graft copolymers were ∼200 000 g/mol and the polydispersity ranged from 1.86 to 2.22. The graft copolymers contained ∼9-10 branches on average and 4 wt % of sulfonic acid or sodium sulfonate blocks adjacent to the backbone or at the branch terminus. The mobility of the sulfonated blocks located at the branch terminus enabled the sulfonated blocks to more readily interact and form ionic aggregates. The glass transition temperatures of the sulfonated graft copolymer with sulfonated blocks at the branch terminus were higher than values for copolymers with sulfonated blocks adjacent to the backbone. This behavior was attributed to the sulfonated blocks at the branch terminus more easily forming ionic aggregates. In general, appearance of multiple scattering maxima in the small-angle X-ray scattering (SAXS) data indicated the formation of lamellar morphologies. More facile aggregation of sulfonated blocks at the branch terminus resulted in the appearance of ionomer peaks in SAXS whereas ionomer peaks were not observed in sulfonated graft copolymers with sulfonated blocks adjacent to the backbone. Reasonable fits of the Yarusso - Cooper model to the SAXS data strongly supported the identification of the nonlamellar maxima as ionomer peaks. Strong ionic interactions with Na+ counterions reduced the Bragg spacings, d, of the sodium sulfonate graft copolymers and increased the size of the ionic aggregates. The location of sulfonated blocks in both sulfonic acid and sodium sulfonate graft copolymers significantly affected thermal properties and morphologies.

元の言語English
ページ(範囲)3503-3512
ページ数10
ジャーナルMacromolecules
41
発行部数10
DOI
出版物ステータスPublished - 2008 5 27
外部発表Yes

Fingerprint

Sulfonation
Graft copolymers
Acrylics
Sulfonic Acids
Ionomers
Sodium
X ray scattering
Acids
Polymethyl Methacrylate
Polymethyl methacrylates
Styrene
Multiple scattering
Polydispersity
Identification (control systems)
Thermodynamic properties
Agglomeration
Copolymers
Salts
Molecular weight

ASJC Scopus subject areas

  • Materials Chemistry

これを引用

Saito, T., Mather, B. D., Costanzo, P. J., Beyer, F. L., & Long, T. E. (2008). Influence of site-specific sulfonation on acrylic graft copolymer morphology. Macromolecules, 41(10), 3503-3512. https://doi.org/10.1021/ma800178d

Influence of site-specific sulfonation on acrylic graft copolymer morphology. / Saito, Tomonori; Mather, Brian D.; Costanzo, Philip J.; Beyer, Frederick L.; Long, Timothy Edward.

:: Macromolecules, 巻 41, 番号 10, 27.05.2008, p. 3503-3512.

研究成果: Article

Saito, T, Mather, BD, Costanzo, PJ, Beyer, FL & Long, TE 2008, 'Influence of site-specific sulfonation on acrylic graft copolymer morphology', Macromolecules, 巻. 41, 番号 10, pp. 3503-3512. https://doi.org/10.1021/ma800178d
Saito T, Mather BD, Costanzo PJ, Beyer FL, Long TE. Influence of site-specific sulfonation on acrylic graft copolymer morphology. Macromolecules. 2008 5 27;41(10):3503-3512. https://doi.org/10.1021/ma800178d
Saito, Tomonori ; Mather, Brian D. ; Costanzo, Philip J. ; Beyer, Frederick L. ; Long, Timothy Edward. / Influence of site-specific sulfonation on acrylic graft copolymer morphology. :: Macromolecules. 2008 ; 巻 41, 番号 10. pp. 3503-3512.
@article{d2465bf7cb904fd09c6530a9edd6b2da,
title = "Influence of site-specific sulfonation on acrylic graft copolymer morphology",
abstract = "Novel selectively sulfonated graft copolymers, poly(methyl methacrylate)-g-(poly(sulfonic acid styrene)-b-poly(tert-butylstyrene)), poly(methyl methacrylate)-g-(poly(tert-butylstyrene)-b-poly(styrenesulfonic acid)), and the corresponding sodium sulfonate salts were successfully synthesized. The weight-average molecular weights (Mw) of the graft copolymers were ∼200 000 g/mol and the polydispersity ranged from 1.86 to 2.22. The graft copolymers contained ∼9-10 branches on average and 4 wt {\%} of sulfonic acid or sodium sulfonate blocks adjacent to the backbone or at the branch terminus. The mobility of the sulfonated blocks located at the branch terminus enabled the sulfonated blocks to more readily interact and form ionic aggregates. The glass transition temperatures of the sulfonated graft copolymer with sulfonated blocks at the branch terminus were higher than values for copolymers with sulfonated blocks adjacent to the backbone. This behavior was attributed to the sulfonated blocks at the branch terminus more easily forming ionic aggregates. In general, appearance of multiple scattering maxima in the small-angle X-ray scattering (SAXS) data indicated the formation of lamellar morphologies. More facile aggregation of sulfonated blocks at the branch terminus resulted in the appearance of ionomer peaks in SAXS whereas ionomer peaks were not observed in sulfonated graft copolymers with sulfonated blocks adjacent to the backbone. Reasonable fits of the Yarusso - Cooper model to the SAXS data strongly supported the identification of the nonlamellar maxima as ionomer peaks. Strong ionic interactions with Na+ counterions reduced the Bragg spacings, d, of the sodium sulfonate graft copolymers and increased the size of the ionic aggregates. The location of sulfonated blocks in both sulfonic acid and sodium sulfonate graft copolymers significantly affected thermal properties and morphologies.",
author = "Tomonori Saito and Mather, {Brian D.} and Costanzo, {Philip J.} and Beyer, {Frederick L.} and Long, {Timothy Edward}",
year = "2008",
month = "5",
day = "27",
doi = "10.1021/ma800178d",
language = "English",
volume = "41",
pages = "3503--3512",
journal = "Macromolecules",
issn = "0024-9297",
publisher = "American Chemical Society",
number = "10",

}

TY - JOUR

T1 - Influence of site-specific sulfonation on acrylic graft copolymer morphology

AU - Saito, Tomonori

AU - Mather, Brian D.

AU - Costanzo, Philip J.

AU - Beyer, Frederick L.

AU - Long, Timothy Edward

PY - 2008/5/27

Y1 - 2008/5/27

N2 - Novel selectively sulfonated graft copolymers, poly(methyl methacrylate)-g-(poly(sulfonic acid styrene)-b-poly(tert-butylstyrene)), poly(methyl methacrylate)-g-(poly(tert-butylstyrene)-b-poly(styrenesulfonic acid)), and the corresponding sodium sulfonate salts were successfully synthesized. The weight-average molecular weights (Mw) of the graft copolymers were ∼200 000 g/mol and the polydispersity ranged from 1.86 to 2.22. The graft copolymers contained ∼9-10 branches on average and 4 wt % of sulfonic acid or sodium sulfonate blocks adjacent to the backbone or at the branch terminus. The mobility of the sulfonated blocks located at the branch terminus enabled the sulfonated blocks to more readily interact and form ionic aggregates. The glass transition temperatures of the sulfonated graft copolymer with sulfonated blocks at the branch terminus were higher than values for copolymers with sulfonated blocks adjacent to the backbone. This behavior was attributed to the sulfonated blocks at the branch terminus more easily forming ionic aggregates. In general, appearance of multiple scattering maxima in the small-angle X-ray scattering (SAXS) data indicated the formation of lamellar morphologies. More facile aggregation of sulfonated blocks at the branch terminus resulted in the appearance of ionomer peaks in SAXS whereas ionomer peaks were not observed in sulfonated graft copolymers with sulfonated blocks adjacent to the backbone. Reasonable fits of the Yarusso - Cooper model to the SAXS data strongly supported the identification of the nonlamellar maxima as ionomer peaks. Strong ionic interactions with Na+ counterions reduced the Bragg spacings, d, of the sodium sulfonate graft copolymers and increased the size of the ionic aggregates. The location of sulfonated blocks in both sulfonic acid and sodium sulfonate graft copolymers significantly affected thermal properties and morphologies.

AB - Novel selectively sulfonated graft copolymers, poly(methyl methacrylate)-g-(poly(sulfonic acid styrene)-b-poly(tert-butylstyrene)), poly(methyl methacrylate)-g-(poly(tert-butylstyrene)-b-poly(styrenesulfonic acid)), and the corresponding sodium sulfonate salts were successfully synthesized. The weight-average molecular weights (Mw) of the graft copolymers were ∼200 000 g/mol and the polydispersity ranged from 1.86 to 2.22. The graft copolymers contained ∼9-10 branches on average and 4 wt % of sulfonic acid or sodium sulfonate blocks adjacent to the backbone or at the branch terminus. The mobility of the sulfonated blocks located at the branch terminus enabled the sulfonated blocks to more readily interact and form ionic aggregates. The glass transition temperatures of the sulfonated graft copolymer with sulfonated blocks at the branch terminus were higher than values for copolymers with sulfonated blocks adjacent to the backbone. This behavior was attributed to the sulfonated blocks at the branch terminus more easily forming ionic aggregates. In general, appearance of multiple scattering maxima in the small-angle X-ray scattering (SAXS) data indicated the formation of lamellar morphologies. More facile aggregation of sulfonated blocks at the branch terminus resulted in the appearance of ionomer peaks in SAXS whereas ionomer peaks were not observed in sulfonated graft copolymers with sulfonated blocks adjacent to the backbone. Reasonable fits of the Yarusso - Cooper model to the SAXS data strongly supported the identification of the nonlamellar maxima as ionomer peaks. Strong ionic interactions with Na+ counterions reduced the Bragg spacings, d, of the sodium sulfonate graft copolymers and increased the size of the ionic aggregates. The location of sulfonated blocks in both sulfonic acid and sodium sulfonate graft copolymers significantly affected thermal properties and morphologies.

UR - http://www.scopus.com/inward/record.url?scp=45749105102&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=45749105102&partnerID=8YFLogxK

U2 - 10.1021/ma800178d

DO - 10.1021/ma800178d

M3 - Article

AN - SCOPUS:45749105102

VL - 41

SP - 3503

EP - 3512

JO - Macromolecules

JF - Macromolecules

SN - 0024-9297

IS - 10

ER -