Low-energy ion scattering from the Si(111) surface: Analysis of the clean 7×7 and Te-stabilized "1×1" structures

M. Aono*, R. Souda, C. Oshima, Y. Ishizawa

*この研究の対応する著者

    研究成果: Article査読

    8 被引用数 (Scopus)

    抄録

    For the clean 7×7 and Te-stabilized "1×1" structures of the Si(111) surface, the following models are proposed on the basis of specialized low-energy ion scattering experiments: The 7×7 and "1×1" structures are constructed by ordered and disoredered pyramidal clusters of adatoms, respectively.