Partial discharge degradation of several biodegradable polymers

Norikazu Fuse, Shinjiro Fujita, Naoshi Hirai, Toshikatsu Tanaka, Masahiro Kozako, Masanori Kohtoh, Shigemitsu Okabe, Yoshimichi Ohki

研究成果: Article

12 引用 (Scopus)

抜粋

Partial discharge (PD) resistance was examined by applying a constant voltage for four kinds of biodegradable polymers, i.e. poly-L-lactic acid (PLLA), polyethylene terephthalate succinate (PETS), poly ε-caprolactone butylene succinate (PCL-BS), and polybutylene succinate (PBS), and the results were compared with those of low density polyethylene (LDPE) and crosslinked low density polyethylene (XLPE). The PD resistance is determined by the erosion depth and the surface roughness caused by PDs, and is ranked as LDPE ≅ XLPE > PLLA ≅ PETS > PBS > PCL-BS. This means that the sample with a lower permittivity has better PD resistance. Furthermore, observations of the sample surface by a polarization microscope and a laser confocal one reveal that crystalline regions with spherulites are more resistant to PDs than amorphous regions. Therefore, good PD resistance can be achieved by the sample with a high crystallinity and a low permittivity.

元の言語English
ジャーナルIEEJ Transactions on Fundamentals and Materials
127
発行部数8
出版物ステータスPublished - 2007

    フィンガープリント

ASJC Scopus subject areas

  • Electrical and Electronic Engineering

これを引用