Stress Corrosion Cracking of Notched GFRP Laminates (Microscopic Fracture Model and Crack Propagation Rate)
Hiroyuki Kawada, Akiyoshi Okada, Hironori Ueno, Ikuhiko Hayashi
研究成果: Article › 査読