The solubility of palladium in the FeO x -SiO 2 slags at 1573K

Ryo Ogasawara, Hidehiro Sekimoto, Katsunori Yamaguchi

研究成果: Paper

抄録

There is an increasing trend in the copper smelters to recycle electronic materials, which contain relatively high concentration of platinum group metals. Platinum group metals lost in the slag is increasing with increasing of treated scrap amount. To determine the portion of the platinum group metals chemically dissolved in the slag will be a key factor to improve the recovery of those metals. An experimental study was carried out to determine the solubility of palladium in the FeOx-SiO 2 slag equilibrated with a pure palladium and the liquid Cu-Pd alloy at 1573 K and the range of oxygen partial pressure from 10 -9 to 10 -7 . The solubility of palladium in the slag tends to increase with increasing oxygen partial pressure and content of copper in the slag. Based on the measured palladium solubility, activity coefficients of palladium oxide in the FeO x -SiO 2 slag were derived. The activity coefficients decrease with increasing copper contents in the slag. Therefore, lower copper content in the slag tend to lower precious metals dissolution in the slag.

元の言語English
出版物ステータスPublished - 2017 1 1
イベント14th International Symposium on East Asian Resources Recycling Technology, EARTH 2017 - Sapporo, Hokkaido, Japan
継続期間: 2017 9 262017 9 29

Conference

Conference14th International Symposium on East Asian Resources Recycling Technology, EARTH 2017
Japan
Sapporo, Hokkaido
期間17/9/2617/9/29

Fingerprint

palladium
slag
solubility
platinum
copper
activity coefficient
metal
partial pressure
oxygen
precious metal
experimental study
dissolution
oxide
liquid

ASJC Scopus subject areas

  • Environmental Science(all)

これを引用

Ogasawara, R., Sekimoto, H., & Yamaguchi, K. (2017). The solubility of palladium in the FeO x -SiO 2 slags at 1573K . 論文発表場所 14th International Symposium on East Asian Resources Recycling Technology, EARTH 2017, Sapporo, Hokkaido, Japan.

The solubility of palladium in the FeO x -SiO 2 slags at 1573K . / Ogasawara, Ryo; Sekimoto, Hidehiro; Yamaguchi, Katsunori.

2017. 論文発表場所 14th International Symposium on East Asian Resources Recycling Technology, EARTH 2017, Sapporo, Hokkaido, Japan.

研究成果: Paper

Ogasawara, R, Sekimoto, H & Yamaguchi, K 2017, ' The solubility of palladium in the FeO x -SiO 2 slags at 1573K ', 論文発表場所 14th International Symposium on East Asian Resources Recycling Technology, EARTH 2017, Sapporo, Hokkaido, Japan, 17/9/26 - 17/9/29.
Ogasawara R, Sekimoto H, Yamaguchi K. The solubility of palladium in the FeO x -SiO 2 slags at 1573K . 2017. 論文発表場所 14th International Symposium on East Asian Resources Recycling Technology, EARTH 2017, Sapporo, Hokkaido, Japan.
Ogasawara, Ryo ; Sekimoto, Hidehiro ; Yamaguchi, Katsunori. / The solubility of palladium in the FeO x -SiO 2 slags at 1573K 論文発表場所 14th International Symposium on East Asian Resources Recycling Technology, EARTH 2017, Sapporo, Hokkaido, Japan.
@conference{ccb8145be19444f58358caedcd8be8ec,
title = "The solubility of palladium in the FeO x -SiO 2 slags at 1573K",
abstract = "There is an increasing trend in the copper smelters to recycle electronic materials, which contain relatively high concentration of platinum group metals. Platinum group metals lost in the slag is increasing with increasing of treated scrap amount. To determine the portion of the platinum group metals chemically dissolved in the slag will be a key factor to improve the recovery of those metals. An experimental study was carried out to determine the solubility of palladium in the FeOx-SiO 2 slag equilibrated with a pure palladium and the liquid Cu-Pd alloy at 1573 K and the range of oxygen partial pressure from 10 -9 to 10 -7 . The solubility of palladium in the slag tends to increase with increasing oxygen partial pressure and content of copper in the slag. Based on the measured palladium solubility, activity coefficients of palladium oxide in the FeO x -SiO 2 slag were derived. The activity coefficients decrease with increasing copper contents in the slag. Therefore, lower copper content in the slag tend to lower precious metals dissolution in the slag.",
keywords = "Activity coefficient, Cu-Pd alloy, Platinum group metals, Slag loss",
author = "Ryo Ogasawara and Hidehiro Sekimoto and Katsunori Yamaguchi",
year = "2017",
month = "1",
day = "1",
language = "English",
note = "14th International Symposium on East Asian Resources Recycling Technology, EARTH 2017 ; Conference date: 26-09-2017 Through 29-09-2017",

}

TY - CONF

T1 - The solubility of palladium in the FeO x -SiO 2 slags at 1573K

AU - Ogasawara, Ryo

AU - Sekimoto, Hidehiro

AU - Yamaguchi, Katsunori

PY - 2017/1/1

Y1 - 2017/1/1

N2 - There is an increasing trend in the copper smelters to recycle electronic materials, which contain relatively high concentration of platinum group metals. Platinum group metals lost in the slag is increasing with increasing of treated scrap amount. To determine the portion of the platinum group metals chemically dissolved in the slag will be a key factor to improve the recovery of those metals. An experimental study was carried out to determine the solubility of palladium in the FeOx-SiO 2 slag equilibrated with a pure palladium and the liquid Cu-Pd alloy at 1573 K and the range of oxygen partial pressure from 10 -9 to 10 -7 . The solubility of palladium in the slag tends to increase with increasing oxygen partial pressure and content of copper in the slag. Based on the measured palladium solubility, activity coefficients of palladium oxide in the FeO x -SiO 2 slag were derived. The activity coefficients decrease with increasing copper contents in the slag. Therefore, lower copper content in the slag tend to lower precious metals dissolution in the slag.

AB - There is an increasing trend in the copper smelters to recycle electronic materials, which contain relatively high concentration of platinum group metals. Platinum group metals lost in the slag is increasing with increasing of treated scrap amount. To determine the portion of the platinum group metals chemically dissolved in the slag will be a key factor to improve the recovery of those metals. An experimental study was carried out to determine the solubility of palladium in the FeOx-SiO 2 slag equilibrated with a pure palladium and the liquid Cu-Pd alloy at 1573 K and the range of oxygen partial pressure from 10 -9 to 10 -7 . The solubility of palladium in the slag tends to increase with increasing oxygen partial pressure and content of copper in the slag. Based on the measured palladium solubility, activity coefficients of palladium oxide in the FeO x -SiO 2 slag were derived. The activity coefficients decrease with increasing copper contents in the slag. Therefore, lower copper content in the slag tend to lower precious metals dissolution in the slag.

KW - Activity coefficient

KW - Cu-Pd alloy

KW - Platinum group metals

KW - Slag loss

UR - http://www.scopus.com/inward/record.url?scp=85065981204&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=85065981204&partnerID=8YFLogxK

M3 - Paper

ER -